HOME > Engineering plastics > Grades and Properties > Xyron grades and properties


PPE/PS Non-Reinforced
DTUL(°C)
1.80MPa
ISO Method
(ASTM Method)
Flammability (UL-94)
HB V-2 V-1 V-0
70
(76)
    1950J
1951J
 
78
(85)
    100V 100Z
83
(90)
200H 240W 240V 240Z
94
(100)
300H 340W 340V 340Z
104
(110)
400H     440Z
-
106
      PV40Z
114
(120)
500H   540V 540Z
124
(130)
600H   640V 640Z
129       644Z
134
(140)
    740V  
144
(150)
      SZ800
164
(170)
1000H
(Eq. to HB)
     
PPE/PS Reinforced
DTUL(°C)
1.80MPa
ISO Method
(ASTM Method)
Flammability
(UL-94)
Glass Fiber High-Stiffness
Low-Warp
High-Flow
High-Stiffness
Low-Warp
High-Stiffness
Ultra Low-Warp
Good Appearance
Low-Warp
Electroconductive
High-Stiffness
Carbon Fiber
Acoustic Damping
97
(100)
HB         X352H    
V-1     X331V
X332V
X1509
X1508
X351V
X352V
  VN30V
VT31V
V-0     X1561       VT31Z
108
(110)
HB     X444H X304H
X404H
     
V-1              
V-0       X1712      
118
(120)
HB         X552H    
V-1   L542V
L543V
X1744
L544V
L554V
L564V
L565V
X531V L524V X551V
X552V
X8610  
V-0   L542Z
L543Z
L564Z
L574Z
X531Z     X8401  
128
(130)
HB G701H     X604H      
V-1 G701V     X603V      
133
(130)
V-1   L654V          
139
(140)
HB G702H
G703H
           
V-1 G702V
G703V
           
PP/PPE
DTUL(°C)
1.80MPa
ISO Method
(ASTM Method)
Flammability
(UL-94)
Non-Reinforced Reinforced
90
(97)
- EV103    
100
(120)
HB     TT520
120
(135)
  T0702  
PA/PPE
DTUL(°C)
1.80MPa
ISO Method
Non-Reinforced Reinforced
80 A0210  
113 AT610  
138   AT602
143 AT600  
150   AG511
180   AG512
199   AG211
226   AG213
PPS/PPE
DTUL(°C)
1.80MPa
ISO Method
Flammability (UL-94)
V-1 V-0
240 DG235  
241 DG141  
262 DV166  
PPE Powder
  Grade
Standard S201A
Low viscosity S202A